Reason 3: The adsorption tower enters a lot of oil or liquid water. The addition of oil will lead to aluminum bead poisoning and loss of adsorption capacity. A lot of liquid water will lead to adsorption failure, dew point temperature rise, and pulverization and crushing will be formed under long-term high pressure.

Reason 4: The equipment has differential pressure. The main reasons for the pulverization and crushing of activated alumina beads are the above. I hope it can help you. The activated alumina sphere is a kind of outstanding solid adsorption material with large pore volume and specific surface area. According to the analysis of the alumina bead manufacturer, the activated alumina bead is a pure aluminum product. The main crystal phase is Y-shaped. There are many internal channels, which are interconnected. The pore size is large, and the specific surface area is large. It is a porous, highly dispersed solid material with outstanding adsorption, pressure resistance, wear resistance and heat resistance. This product has uniform particles, lubricated surface, high mechanical strength, strong moisture absorption capacity, no swelling or cracking when absorbing water, and adheres to the original state. It is non-toxic, odorless, insoluble in water, and alcohol free. It is harmless to human body and the surrounding environment. It is widely used in petrochemical, fertilizer, steel and other professions.